Modulus Of Rupture:1.5MPa
Working Temperature:1450℃
Compressive Strength:≥50MPa
Working Temperature:High
Acid Resistance:High
Size:230x114x65 mm
Al2O3 Content (%):48%-85%
MgO Content (%):0.8-1.2
CaO Content (%):0.34%
Impact Resistance:High
Carbon Content:≤1.5%
Application Temperature:Above 1500℃
Origin:Xinmi
Refractoriness Under Load:≥ 1470℃
Resistance To Corrosion:Excellent
Apparent Porosity:≤ 22%
Density:2.2-2.4 g/cm3
Item:high alumina brick
Service Life:Long
Bulk Density:≥ 2.5 g/cm3
Cold Crushing Strenghth:60 Mpa
Alkali Resistance:High
Durability:High
Impact Resistance:High
Service Life:Long
Compressive Strength:≥45MPa
Impact Resistance:High
Carbon Content:≤1.5%
Application:High temperature industrial furnaces and kilns
Size:Customers' Requirement
Resistance To Corrosion:Excellent
Heat Resistance:High
Mohs Hardness:7-8
Thermal Shock Resistance:Good
Shape:Rectangular, square, or customized
Acid Resistance:High